1.C. C. Xue, Z. Y. Zhang, J. B. Tan, X. Q. Wu, E.-H. Han, W. Ke, Effects of Zn injection on corrosion behavior and crud deposition of FeCrAl fuel cladding under subcooled nuclear boiling condition in high-temperature pressurized water, Corrosion Science, 211 (2023) 110909

2.B. Q. Xue, J. B. Tan, Z. Y. Zhang, X. Wang, X. Q. Wu, E.-H. Han, W. Ke, Effect of temperature on low cycle fatigue behavior of T91 steel in liquid lead-bismuth eutectic environment at 150-550 , International Journal of Fatigue, 167 (2023) 107344

3.S.Z. Zhang, X.B. Shi, Y. Liang, H.T. Xu, C.G Yan, W. Yan, L. J. Rong, K. Yang, phase and its effect on the mechanical properties of a Mo-bearing high–Si austenitic stainless steel after aging at 650 , Journal of Materials Research and Technology, 23 (2023) 4280-4292

4.Pengxiang Zhao, Xiaobing Li, Weiwei Xing, Bo Chen, Yingche Ma, Kui Liu, Cyclic oxidation behavior of Nb/Mn/Si alloying Beta?Gamma TiAl alloys, Transactions of Nonferrous Metals Society of China, 33 (2023) 128-140

5.B. W. Zhao, Y. L. Liu, H. Zhang, S. T. Li, G. F. Ma, S. M. Zhang, H. F. Zhang, Z. W. Zhu, In-situ activation of Fe78Si9B13 metallic glasses for electro-Fenton degradation of industrial oily wastewater, Sustainable Materials and Technologies, 35 (2023) e00539

6.T. Y. Yan, L. Zhang, R. L. Narayan, J. Y. Pang, Y. Wu, H. M. Fu, H. Li, U. Ramamurty, H. F. Zhang, Effects of Al addition and cryogenic cyclic treatment on impact toughness of phase-transformable Ti-based bulk metallic glass composites, Journal of Materials Science & Technology, 140 (2023) 210-220

7.M. L. Liu, W. Li, S. Zeng, Y. F. Li, H. M. Fu, H. Li, A. M. Wang, X. P. Lin, H. F. Zhang, Z. W. Zhu, Ductilizing Ti19Zr19Hf19Nb19TM5Be19 (TM = Fe, Co, Ni and Cu) high-entropy bulk metallic glass composites via in-situ precipitated refractory high-entropy alloy dendrites, Intermetallics, 152 (2023) 107755

8.Yusheng Zhang, Jiang Lai, Jiazhen Wang, Lixia Gao, Hongliang Ming, Jianqiu Wang, En-Hou Han, Establishment of fretting maps of Zr alloy cladding tube mated with Zr alloy dimple in simulated primary water of pressurized water reactor, Tribology International, 178 (2023) 108065

9.S. H. Chen, A. Xie, X. L. Lv, S. H. Chen, C. G. Yan, H. C. Jiang, L. J. Rong, Tailoring microstructure of austenitic stainless steel with improved performance for generation-IV fast reactor application: A review, Crystals, 13 (2023) 268

10.J. Ma, X. C. Liu, D. S. Yan, L. J. Rong, A novel GP-Li precursor and the correlated precipitation behaviors in Al-Cu-Li alloys with different Cu/Li ratio, Acta Materialia, 243 (2023) 118442

11.S. Z. Zhang, X. B. Shi, Y. Liang, H. T. Xue, C. G. Yan, W. Yan, L. J. Rong, K. Yang, phase and its effect on the mechanical properties of a Mo-bearing high-Si austenitic stainless steel after aging at 650 , Journal of Materials Research and Technology, 23 (2023) 4280-4292

12.J. X. Liu, M. J. Zhao, L. J. Rong, Overview of hydrogen-resistant alloys for high-pressure hydrogen environment: on the hydrogen energy structural materials, Clean Energy, 7 (2023) 99-115

13.W. B. Tian, W.C. Dong, S.P. Lu, Microstructure evolution and mechanical properties of 16Cr-25Ni superaustenitic stainless steel weld metal during 600 aging, Journal of Materiasl Research and Technology, 22 (2023) 461-472

14.陆善平,徐海涛,吴栋,燕春光,陈亚魁,韩丽青,戎利建,庄毅,杨红义,李依依,一种调控含Nb不锈钢焊缝金属 铁素体和碳化物的方法,ZL202211238605.5

15.赵明久,刘家兴,姜海昌,戎利建,一种牌号为MP-5的高强度耐氢脆膜片及制备方法,ZL202111223294.0

16.赵明久,刘家兴,姜海昌,戎利建,一种高压氢压机膜片用耐疲劳耐氢脆板材的制备方法,ZL202111230291.X

17.赵明久,刘家兴,姜海昌,戎利建,一种牌号为MP-7的高强度耐氢脆膜片及制备方法,ZL202111221854.9

18.姜海昌,胡小锋,潘雪新,戎利建,周平宇,张洋鹏,李忠文,乔青峰,王旭,徐忠宣,一种高性能轴套材料及其热处理方法,ZL201911185909.8